Call Us Today: 800-523-1266

103 Queens Drive | King of Prussia, PA

            ISO 9001:2015 Certified

ERCuSi-A

Class: ERCuSi-A

AWS: A5.7

Conforms to Certification: AWS – 5.7                   ASME SFA  A5.7

Silicon Bronze: Mig Welding Process (GMAW)

AWS Chemical Composition Requirements
Cu = Remainder Zn = 1.0 max
Sn = 1.0 max Mn = 1.5 max
Fe = 0.50 max Si = 2.8 – 4.0
Al = 0.01 max Pb = 0.02 max
Other = 0.50 max

 

Available Sizes 
Diameter X Spool Sizes Diameter X Coil Sizes
.035 x 30# 1/16 x 60#
.045 x 30# 3/32 x 60#
1/16 x 30# 1/8 x 60#

Application
Use for welding of Silicon Bronze Copper, or Aluminum Bronze of low aluminum content. It can also be used for brazing malleable iron and light gauge steel.

Deposited Chemical Composition % (Typical)
Dependent on weld process

(Nominal) All Weld Metal Properties Requirements
Tensile Strength                                          50,000 psi

Recommended Welding Parameters     
Process Diameter of Wire Voltage (V) Amperage (A) Gas Feed
MIG .035 inches 20-26 100-200 100% Argon or 75% Argon, 25% Helium 45-55 CFH
GMAW (DCEP) .045 inches 22-28 100-200 100% Argon or 75% Argon, 25% Helium 45-55 CFH
1/16 inches 29-32 250-400 100% Argon or 75% Argon, 25% Helium 45-55 CFH
3/32 inches 32-34 350-500 100% Argon or 75% Argon, 25% Helium 45-55 CFH

Preheat / Interpass Recommendations
Preheating copper – base alloys is frequently unnecessary provided section thicknesses are not unusually heavy.
Preheat and Interpass temperatures will vary depending on section thickness, selected weld process and other variables.