Class: ENiFe-CI
AWS: A5.15
Conforms to Certification: AWS A5.15 ASME SFA A5.15
Weld Process: Shielded Metal Arc Weld Process (SMAW)
AWS Chemical Composition Requirements | |
C = 2.0 max | Fe = Remainder |
Mn = 2.5 max | Ni = 45.0 – 60.0 |
Si = 4.0 max | Cu = 2.5 max |
S = 0.03 max | Al = 1.0 max |
Other = 1.0 max |
Available Sizes
3/32
1/8
5/32
3/16
Application
Nickel 55 electrode is designed for welding of cast iron to themselves, as well as joining them to mild steels and repair of castings. Preheat and interpass of 350ºF minimum is recommended during welding.
Deposited Chemical Composition % (Typical) | ||
C = 0.90 | Mn = 0.75 | Si = 2.10 |
Fe = 40.2 | Cu = 1.90 | Ni = 54.5 |
S = 0.006 | P = 0.012 |
Deposited All Weld Properties % (AW) | |
Tensile Strength | 84,000 psi |
Yield Strength | 59,500 psi |
Elongation | 9% |
Deposited Charpy-V-Notch Impact Properties %
Not applicable
Recommended Weld Parameters | Amperage (A) | ||
Diameter of Wire | Voltage (V) | Flat | Vertical and Overhead |
3/32 inches (2.4mm) | 24 – 28 | 70 – 85 | 65 – 75 |
1/8 inches (3.2mm) | 26 – 30 | 85 – 110 | 80 – 90 |
5/32 inches (4.0mm) | 28 – 32 | 110 – 140 | 100 – 120 |
3/16 inches (4.8mm) | 28 – 32 | 120 – 160 | 110 – 130 |