Class: ER316L
AWS: A5.9
Conforms to Certification: AWS A5.9 ASME SFA A5.9
Weld Process Used for Tig (GTAW)
AWS Chemical Composition Requirements
C = 0.03 max
Cr = 18.0 – 20.0
Ni = 11.0 – 14.0
Mo = 2.0 – 3.0
Mn = 1.0 – 2.5
Si = 0.30 – 0.65
P = 0.03 max
S = 0.03 max
Cu = 0.75 max
Available Sizes
.030 x 36
.035 x 36
.045 x 36
1/16 x 36
3/32 x 36
1/8 x 36
3/16 x 36
5/32 x 36
Application
ER316L filler metal is primarily used for welding low carbon molybdenum-bearing austenitic alloys. This low carbon alloy is not as strong at elevated temperatures as ER316H.
Deposited Chemical Composition % (Typical) | ||
C = 0.015 | Mo = 2.50 | P = 0.010 |
Cr = 18.75 | Mn = 1.80 | S = 0.010 |
Ni = 12.25 | Si = 0.34 |
Mechanical Properties (R.T.) | |
Yield Strength | 59,000psi |
Tensile Strength | 88,000psi |
Elongation | 35% |
Reduction of Area | 39% |
Deposited All Weld Metal Properties
Data is typical for ER316L weld metal deposited by Tig using 100% Argon as the shielding gas.
Recommended Welding Parameters | |||
GTAW “Tig Process” | |||
Wire Diameter | Amps DCSP | Volts | Shielding Gas |
.035 | 60-90 | 12-15 | Argon 100% |
.045 | 80-110 | 13-16 | Argon 100% |
1/16 | 90-130 | 14-16 | Argon 100% |
3/32 | 120-175 | 15-20 | Argon 100% |
Note: Parameters for tig welding are dependent upon plate thickness and welding position.