Call Us Today: 800-523-1266

103 Queens Drive | King of Prussia, PA

            ISO 9001:2015 Certified

ER347

Class: ER347

AWS: A5.9

Conforms to Certification: AWS A5.9               ASME SFA A5.9

Weld Process Used for Tig (GTAW)

AWS Chemical Composition Requirements
C = 0.08 max
Cr = 19.0 – 21.5
Ni = 9.0 – 11.0
Mo = 0.75 max
Mn = 1.0 – 2.5
Si = 0.30 – 0.65
P = 0.03 max
S = 0.03 max
Cu = 0.75 max
Nb = 10 x C (min) – 1.0 (max)

Available Sizes
.030 x 36
.035 x 36
.045 x 36
1/16 x 36
3/32 x 36
1/8 x 36
3/16 x 36
5/32 x 36

Application
ER347 is recommended for welding AISI 347 and 321. The weld metal has good resistance to general corrosion. ER347 is suitable for applications where welds are subjected to high temperatures (+ 750ºF).

Deposited Chemical Composition % (Typical)
C = 0.04 Mo = 0.30 P = 0.025
Cr = 19.50 Mn = 1.30 S = 0.015
Ni = 9.50 Si = 0.40 Cu = 0.10
Nb = 0.40

 

Mechanical Properties (R.T.) 
Yield Strength 88,000psi
Tensile Strength 58,000psi
Elongation 42%

Deposited All Weld Metal Properties
Data is typical for ER347 weld metal deposited by Tig using 100% Argon as the shielding gas.

Recommended Welding Parameters
GTAW “Tig Process”
Wire Diameter Amps DCSP Volts Shielding Gas
.035 60-90 12-15 Argon 100%
.045 80-110 13-16 Argon 100%
1/16 90-130 14-16 Argon 100%
3/32 120-175 15-20 Argon 100%

Note: Parameters for tig welding are dependent upon plate thickness and welding position.
Other shielding Gases may be used for Tig welding. Shielding gases are chosen taking Quality, Cost, and Operability into consideration.