ERNiCrMo-9

Class: ERNiCrMo-9

AWS: A5.14

Conforms to Certification: AWS A5.14         ASME SFA A5.14

Weld Process: GTAW Welding Process

AWS Chemical Composition Requirements
C = 0.015 max Cu = 1.5 – 2.5
Mn = 1.0 max Ni = Remainder
Fe = 18.0 – 21.0 Co = 5.0 max
P = 0.04 max Cr = 21.0 – 23.5
S = 0.03 max Nb + Ta = 0.50 max
Si = 1.0 max Mo = 6.0 – 8.0
W = 1.5 max Other = 0.50 max

Please Call For More Information and Available Sizes

Application
ERNiCrMo-9 is used for welding nickel-chromium-molybdenum base materials to themselves, steel and other nickel base alloys, and for cladding steels.

Deposited Chemical Composition % (Typical)
C = 0.01 Cr = 22.0 Ni = Balance
Cu = 2.0 Mo = 7.1 Fe = 20.5
Co = 2.75

 

Deposited All Weld Metal Properties % (AW) 
Tensile Strength 96,000 psi
Elongation 29%

Deposited Charpy-V-Notch Impact Properties %
Not applicable

Recommended Welding Parameters for TIG, MIG, and SAW Welding of Nickel Alloys
Process Diameter of Wire Voltage (V) Amperage (A) Gas
Tig .035 inches x 36 12 – 15 60 – 90 100% Argon
.045 inches x 36 13 – 16 80 – 110 100% Argon
1/16 inches x 36 14 – 18 90 – 130 100% Argon
3/32 inches x 36 15 – 20 120 – 175 100% Argon
1/8 inches x 36 15 – 20 150 – 220 100% Argon

Note:  Other shielding Gases may be used for Tig welding. Shielding gases are chosen taking Quality, cost, and Operability into consideration.
Note:  Both agglomerated and fused fluxes can be used for submerged arc welding.
Note: The chemical composition of the flux mainly affects the chemistry of the weld metal and consequently its corrosion resistance and mechanical properties.